Influence of TiO2 Content and Basicity Level on the Metallogenic Regularity of V-Ti Sinter
-
摘要: 为了考察不同TiO2含量和碱度水平对钒钛烧结技术经济指标和钒钛烧结矿冶金性能的影响,以便确定更优的烧结和高炉物料结构,为此开展了降低烧结矿TiO2含量,同时提高烧结矿碱度水平的试验研究。研究表明:随着钒钛烧结矿TiO2含量的降低和碱度水平升高,烧结矿各项技术指标明显改善,当烧结矿中TiO2含量从6.0%降低至0.5%,碱度水平从2.0提高至2.5时,成品率提高5.21个百分点,转鼓强度提高5.60个百分点,利用系数较基准期提高25%以上。Abstract: In order to investigate the influence of different TiO2 content and basicity level on the technical and economic indexes of V-Ti sintering and the metallurgical properties of V-Ti sinter,so as to determine a better sintering and blast furnace material mixture,an experimental study was carried out to reduce the TiO2 content of sinter and increase the basicity level of sinter.Experimental results show that with the decrease of TiO2 content and the increase of basicity of V-Ti sinter,the technical indexes of sinter are improved significantly.When the content of TiO2 in sinter decreases from 6.0% to 0.5% and the basicity level is increased from 2.0 to 2.5,the yield is increased by 5.21%,the drum strength is increased by 5.60%,and the utilization coefficient is increased by more than 25% compared with those of the reference period.
-
Key words:
- V-Ti sinter /
- TiO2 content /
- basicity level /
- metallogenic regularity /
- perovskite
点击查看大图
计量
- 文章访问数: 9
- HTML全文浏览量: 2
- PDF下载量: 1
- 被引次数: 0