Zhang Qiang, Li Yangzhou, Chen Liang, Huang Yuming, Xu Huabin. Production Practice on Control of Purity for Cord Steel in Pangang[J]. IRON STEEL VANADIUM TITANIUM, 2013, 34(5): 52-57. doi: 10.7513/j.issn.1004-7638.2013.05.011
Citation: Zhang Qiang, Li Yangzhou, Chen Liang, Huang Yuming, Xu Huabin. Production Practice on Control of Purity for Cord Steel in Pangang[J]. IRON STEEL VANADIUM TITANIUM, 2013, 34(5): 52-57. doi: 10.7513/j.issn.1004-7638.2013.05.011

Production Practice on Control of Purity for Cord Steel in Pangang

doi: 10.7513/j.issn.1004-7638.2013.05.011
  • Received Date: 2013-06-13
  • Due to the extremely strict requirements on the control of [S],[N],[O] and [Ti] content in molten steel,tire cord steel is a kind of wire rods difficult to be produced. Pangang Vanadium Recovery and Steelmaking plant steelmake using hot metal with containing [V]and [Ti],the hot metal heat source is insufficient,and the elemente of [P]and [S]content is higher,so make the process of controlling cord steel production more difficult。Usually,using hot metal desulphurization control the content of [S] under 0.005%,though extending oxygen blowing time 3~5 min in the process of extract vanadium converter,can make the content of [Ti] below 0.003% in the semisteel,in the process of converter,controlling the end-point oxygen activity and the LF process refining using slag formation of reasonable slagging,RH vacuum treatment,can produce meetting the requirements of GB/T 10561-2005 steel cord.
  • loading
  • 加载中

Catalog

    通讯作者: 陈斌, bchen63@163.com
    • 1. 

      沈阳化工大学材料科学与工程学院 沈阳 110142

    1. 本站搜索
    2. 百度学术搜索
    3. 万方数据库搜索
    4. CNKI搜索

    Article Metrics

    Article views (11) PDF downloads(1) Cited by()
    Proportional views
    Related

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return