Qing Jiasheng, Duan Xiangdong, Xiao Mingfu, Liu Qing. Research on Resulfurization Control during Converter Tapping Process[J]. IRON STEEL VANADIUM TITANIUM, 2014, 35(6): 75-80. doi: 10.7513/j.issn.1004-7638.2014.06.015
Citation:
Qing Jiasheng, Duan Xiangdong, Xiao Mingfu, Liu Qing. Research on Resulfurization Control during Converter Tapping Process[J]. IRON STEEL VANADIUM TITANIUM, 2014, 35(6): 75-80. doi: 10.7513/j.issn.1004-7638.2014.06.015
Qing Jiasheng, Duan Xiangdong, Xiao Mingfu, Liu Qing. Research on Resulfurization Control during Converter Tapping Process[J]. IRON STEEL VANADIUM TITANIUM, 2014, 35(6): 75-80. doi: 10.7513/j.issn.1004-7638.2014.06.015
Citation:
Qing Jiasheng, Duan Xiangdong, Xiao Mingfu, Liu Qing. Research on Resulfurization Control during Converter Tapping Process[J]. IRON STEEL VANADIUM TITANIUM, 2014, 35(6): 75-80. doi: 10.7513/j.issn.1004-7638.2014.06.015
1. School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, State Key Laboratory of Advanced Metallurgy, Beijing 100083, China;
2. Pangang Group Xichang Iron & Steel Co., Ltd., Xichang 615000, Sichuan, China;
3. Panzhihua Iron and Steel Group Co., Ltd, Panzhihua 617067, Sichuan, China
With the development of high grade steels,it becomes more and more difficult for BOF to pro-duce low sulfur steel.At present main factors causing resulfurization during semi steel smelting process in Pangang Group Xichang Iron&Steel Company are incomplete skimming desulfurization slag,contribution of auxiliary materials and unsuitable smelting slag composition.After optimizing,desulfurization slag skim-ming procedure,controlling feeding materials quality,improving smelting process and slag washing desul-furization during tapping,average resulfurization reduces from 0.003% down to 0.001%.