Volume 43 Issue 1
Mar.  2022
Turn off MathJax
Article Contents
Duo Yunxia, Wang Lijuan, Li Yi, Wei Zhizhong. Source analysis and control technology of impurity Al in titanium sponge[J]. IRON STEEL VANADIUM TITANIUM, 2022, 43(1): 36-39. doi: 10.7513/j.issn.1004-7638.2022.01.006
Citation: Duo Yunxia, Wang Lijuan, Li Yi, Wei Zhizhong. Source analysis and control technology of impurity Al in titanium sponge[J]. IRON STEEL VANADIUM TITANIUM, 2022, 43(1): 36-39. doi: 10.7513/j.issn.1004-7638.2022.01.006

Source analysis and control technology of impurity Al in titanium sponge

doi: 10.7513/j.issn.1004-7638.2022.01.006
  • Received Date: 2021-07-29
  • Accepted Date: 2022-01-07
  • Available Online: 2022-04-24
  • Publish Date: 2022-02-28
  • The sources of impurity Al in titanium sponge produced by the Kroll process were analyzed. The impurity Al is mainly derived from titanium tetrachloride and magnesium. Based on the source analysis of Al in titanium tetrachloride, water vapor was introduced for Al removal from titanium tetrachloride during the chlorination process, where 84.22% of Al removal ratio can be obtained at 10 kg/h of water dosage. At the same time, Al in magnesium was removed by adding refining agent, and a favorable effect can be obtained at 20 kg/t of refining agent amount. Influenced by the reaction process for titanium sponge formation, Al is not evenly distributed in titanium sponge. Therefore, it is necessary to carry out Al removal measures from the source materials to produce high-quality titanium sponge.
  • loading
  • [1]
    邓国珠, 王武育. 钛冶金[M]. 北京: 冶金工业出版社, 2010.

    Deng Guozhu, Wang Wuyu. Titanium metallurgy[M]. Beijing: Metallurgical Industry Press, 2010.
    [2]
    佟程程. 联合法海绵钛生产中杂质来源及控制办法[D]. 沈阳: 东北大学, 2016.

    Tong Chengcheng. The source of impurity and control measure in the combined process of sponge titanium production[D]. Shenyang: Northeastern University, 2016.
    [3]
    宋光林. 精四氯化钛中主要杂质的分析及其工艺控制技术研究[D]. 北京: 北京理工大学, 2017.

    Song Guanglin. Analysis and control of main impurities in refined titanium tetrachloride[D]. Beijing: Beijing Institute of Technology, 2017.
    [4]
    Shi Yuying, Zhou Yunying, Chen Yinzhi, et al. Source and harm of aluminum trichloride in titanium tetrachloride[J]. Sichuan Metallurgy, 2015,37(2):20−23,40. (石玉英, 周云英, 陈映志, 等. 四氯化钛中三氯化铝的来源及其危害[J]. 四川冶金, 2015,37(2):20−23,40. doi: 10.3969/j.issn.1001-5108.2015.02.006
    [5]
    Zhang Wencheng. Refining method of magnesium[J]. Light Metal, 1991,(2):47−49. (张文成. 镁的精炼方法[J]. 轻金属, 1991,(2):47−49.
    [6]
    陈建立, 刘红斌, 石森森,等. 一种四氯化钛气相中去除三氯化铝的装置: 中国, CN202021182479.2[P].2021-03-16.

    Chen Jianli, Liu Hongbin, Shi Sensen, et al. A device for removing aluminum trichloride from titanium tetrachloride gas phase: China, 202021182479[P]. 2021-03-16.
  • 加载中

Catalog

    通讯作者: 陈斌, bchen63@163.com
    • 1. 

      沈阳化工大学材料科学与工程学院 沈阳 110142

    1. 本站搜索
    2. 百度学术搜索
    3. 万方数据库搜索
    4. CNKI搜索

    Figures(1)  / Tables(4)

    Article Metrics

    Article views (172) PDF downloads(52) Cited by()
    Proportional views
    Related

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return