Cao Xiaoen, Hong Lukuo, Zhou Hemin, Tang Xiaofang, Qi Yuanhong. Research on Recovery of Iron from Natural-basicity Carbon-containing Pellets of Jarosite Residue[J]. IRON STEEL VANADIUM TITANIUM, 2016, 37(5): 84-90. doi: 10.7513/j.issn.1004-7638.2016.05.016
Citation:
Cao Xiaoen, Hong Lukuo, Zhou Hemin, Tang Xiaofang, Qi Yuanhong. Research on Recovery of Iron from Natural-basicity Carbon-containing Pellets of Jarosite Residue[J]. IRON STEEL VANADIUM TITANIUM, 2016, 37(5): 84-90. doi: 10.7513/j.issn.1004-7638.2016.05.016
Cao Xiaoen, Hong Lukuo, Zhou Hemin, Tang Xiaofang, Qi Yuanhong. Research on Recovery of Iron from Natural-basicity Carbon-containing Pellets of Jarosite Residue[J]. IRON STEEL VANADIUM TITANIUM, 2016, 37(5): 84-90. doi: 10.7513/j.issn.1004-7638.2016.05.016
Citation:
Cao Xiaoen, Hong Lukuo, Zhou Hemin, Tang Xiaofang, Qi Yuanhong. Research on Recovery of Iron from Natural-basicity Carbon-containing Pellets of Jarosite Residue[J]. IRON STEEL VANADIUM TITANIUM, 2016, 37(5): 84-90. doi: 10.7513/j.issn.1004-7638.2016.05.016
Jarosite residue is a solid waste originating from iron removal process of zinc hydrometallurgy,containing a certain amount of Fe and other valuable metals.In order to recovery Fe,the rotary hearth furnace direct reduction-melting process had been developed to process carbon-containing pellets of jarosite residue.The effect of the process parameters on Fe recovery from jarosite residue was studied,through direct reduction of natural basicity carbon-containing pellets of jarosite residue.At the same time,the pilot plant test has been carried out with rotary hearth furnace.The optimum conditions from experimental test are as follows:reduction temperature of 1 100℃,reduction time of 30 min,C/O=1.2.Under these conditions,the metallization rate of carbon-containing pellets of jarosite residue reaches 90.6%,the metallization rate of pilot plant test is 75%,the comprehensive recovery rate of iron is 85%.