Zhao Sanchao. Preparation and Characterization of Ti4O7 by Thermal Reduction of Titanium Powder with TiO2[J]. IRON STEEL VANADIUM TITANIUM, 2018, 39(2): 69-73. doi: 10.7513/j.issn.1004-7638.2018.02.011
Citation:
Zhao Sanchao. Preparation and Characterization of Ti4O7 by Thermal Reduction of Titanium Powder with TiO2[J]. IRON STEEL VANADIUM TITANIUM, 2018, 39(2): 69-73. doi: 10.7513/j.issn.1004-7638.2018.02.011
Zhao Sanchao. Preparation and Characterization of Ti4O7 by Thermal Reduction of Titanium Powder with TiO2[J]. IRON STEEL VANADIUM TITANIUM, 2018, 39(2): 69-73. doi: 10.7513/j.issn.1004-7638.2018.02.011
Citation:
Zhao Sanchao. Preparation and Characterization of Ti4O7 by Thermal Reduction of Titanium Powder with TiO2[J]. IRON STEEL VANADIUM TITANIUM, 2018, 39(2): 69-73. doi: 10.7513/j.issn.1004-7638.2018.02.011
In this paper,thermodynamic calculation and analysis are carried out for preparation Ti4O7.With the help of differential thermal-thermal gravimetric analysis,the technological conditions for preparing Ti4O7 with titanium powder as reductant are explored,the sintering temperature is 850 ℃ and the sintering time is 4 ~6 h.Testing and analyzing the thermal stability,XRD,particle size,conductivity and specific surface area of Ti4O7.which provided the reference and basis for the preparation of Ti4O7.