Du Changkun, Mai Jichang, Luo Qingming, Yuan Xiaoli, Wan Xin, Liu Hao. Experimental Research on Use of V-bearing Titaniferous Magnetite for Sintering in Desheng Chuangang Steel[J]. IRON STEEL VANADIUM TITANIUM, 2012, 33(2): 62-66.
Citation:
Du Changkun, Mai Jichang, Luo Qingming, Yuan Xiaoli, Wan Xin, Liu Hao. Experimental Research on Use of V-bearing Titaniferous Magnetite for Sintering in Desheng Chuangang Steel[J]. IRON STEEL VANADIUM TITANIUM, 2012, 33(2): 62-66.
Du Changkun, Mai Jichang, Luo Qingming, Yuan Xiaoli, Wan Xin, Liu Hao. Experimental Research on Use of V-bearing Titaniferous Magnetite for Sintering in Desheng Chuangang Steel[J]. IRON STEEL VANADIUM TITANIUM, 2012, 33(2): 62-66.
Citation:
Du Changkun, Mai Jichang, Luo Qingming, Yuan Xiaoli, Wan Xin, Liu Hao. Experimental Research on Use of V-bearing Titaniferous Magnetite for Sintering in Desheng Chuangang Steel[J]. IRON STEEL VANADIUM TITANIUM, 2012, 33(2): 62-66.
In view that high proportion of V-bearing titaniferous magnetite is used at the sinter plant of Sichuan Desheng Iron and Steel Co.,effects of proportioning of V-bearing titaniferous magnetite and basicity on sinter performance were investigated in the lab.The results show that in order to meet the requirement of productivity and quality of sinter,save energy and reduce cost based on the existing raw material,fuel and ore matching in Chuanggang,the desirable proportion of V-bearing titaniferous magnetite is 45% and reasonable basicity is 2.3.