Dou Zhiyong, Huang Bin, Feng Shaoqiang. Analysis and Countermeasures of Bulging Defect at the Edge of Cold-rolled Products[J]. IRON STEEL VANADIUM TITANIUM, 2012, 33(6): 91-94.
Citation: Dou Zhiyong, Huang Bin, Feng Shaoqiang. Analysis and Countermeasures of Bulging Defect at the Edge of Cold-rolled Products[J]. IRON STEEL VANADIUM TITANIUM, 2012, 33(6): 91-94.

Analysis and Countermeasures of Bulging Defect at the Edge of Cold-rolled Products

  • Received Date: 2012-07-19
    Available Online: 2023-12-04
  • Bulging defects at the edge of strip steel forming during cold rolling process and corresponding measuring data are analyzed.It is concluded that local high spots at hot rolled strip steel are the major causes of the defects.In addition,convexity and wedge of the hot rolled plates and rolling length have certain influence on the formation of defects.Causes of local high spots are analyzed in the aspects of microstructure and rolling stress,and finally the bulging defects are noticeably reduced through process improvement.
  • loading
  • 加载中

Catalog

    通讯作者: 陈斌, bchen63@163.com
    • 1. 

      沈阳化工大学材料科学与工程学院 沈阳 110142

    1. 本站搜索
    2. 百度学术搜索
    3. 万方数据库搜索
    4. CNKI搜索

    Article Metrics

    Article views (21) PDF downloads(1) Cited by()
    Proportional views
    Related

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return