PENG Mingfu, ZHU Shengyou, CENG Zhiyong, DENG Xiaobo, TANG Hongguo. OPTIMIZATION OF BURDEN CONSTITUENTS FOR ROASTING VANADIUM SLAG PRODUCED IN CONVERTER IN MULTI-HEARTH ROASTER[J]. IRON STEEL VANADIUM TITANIUM, 1998, 19(4): 36-40.
Citation:
PENG Mingfu, ZHU Shengyou, CENG Zhiyong, DENG Xiaobo, TANG Hongguo. OPTIMIZATION OF BURDEN CONSTITUENTS FOR ROASTING VANADIUM SLAG PRODUCED IN CONVERTER IN MULTI-HEARTH ROASTER[J]. IRON STEEL VANADIUM TITANIUM, 1998, 19(4): 36-40.
PENG Mingfu, ZHU Shengyou, CENG Zhiyong, DENG Xiaobo, TANG Hongguo. OPTIMIZATION OF BURDEN CONSTITUENTS FOR ROASTING VANADIUM SLAG PRODUCED IN CONVERTER IN MULTI-HEARTH ROASTER[J]. IRON STEEL VANADIUM TITANIUM, 1998, 19(4): 36-40.
Citation:
PENG Mingfu, ZHU Shengyou, CENG Zhiyong, DENG Xiaobo, TANG Hongguo. OPTIMIZATION OF BURDEN CONSTITUENTS FOR ROASTING VANADIUM SLAG PRODUCED IN CONVERTER IN MULTI-HEARTH ROASTER[J]. IRON STEEL VANADIUM TITANIUM, 1998, 19(4): 36-40.
Because the burden constituents is not rational in roasting vanadium slag produced in converter in multi-hearth roaster, there are problems such as rake adhering and material adhesion.Therefore, the optimization of burden constituents was conducted, making it smooth to roast the vanadium slag in multi-hearth roaster at≤800℃. which is benefit to improve recovery of vanadium in the slag roasted.