Vanadium Distribution between Slag and Iron at Blow End Point and Its Phase Analysis
-
摘要: 采用具备顶底复吹功能的500 kg中频感应炉模拟复吹转炉铁水提钒工艺,研究吹炼终点钒在渣铁间的分配比;运用X射线衍射分析钒铁尖晶石的分子组成。试验结果表明:吹炼终点钒在渣铁间分配比Lv为1.8~2.8,且与渣中FeO含量相关。为了保证钒渣质量,降低钒渣中FeO含量,减少铁损,吹炼终点V的质量分数不宜过低。钒渣中钒铁尖晶石的分子式为FeO(Fe,V)2O3,表明钒渣中钒为+3价。吹炼初期钒渣中存在少量+2价钒,随着供氧量增加,+2价钒的数量逐渐减少。Abstract: The vanadium extraction in combination blowing converter was simulated by 500 kg scale intermediate frequency induction furnace with top and bottom combinational blowing function,and the vanadium distribution(Lv) between iron and slag phase at blow end point was investigated. The compositions of vanadium-iron spinel were also analyzed by X-ray diffraction(XRD).The results show that vanadium distribution Lv between slag and iron at the blow end point is 1.8~2.8,which is related to the FeO content in slag.To ensure the quality of vanadium slag and decrease the FeO content with lower iron loss,the content of vanadium at the blow end point should be controlled at an appropriate high level. The formula of vanadium-iron spinel in vanadium slag was Fe O(Fe,V)2O3 indicating +3 for the valence of vanadium in slag phase.A small amount of V2+ species was evidenced to exist in the vanadium slag at the initial stage of blowing and gradually decreased with increase in oxygen supply.
-
计量
- 文章访问数: 191
- HTML全文浏览量: 50
- PDF下载量: 6
- 被引次数: 0
下载: